Suburban street repaving crew at work
Asphalt Guide

Asphalt Mix Types Explained: What Sizes 7, 10, 14 and 20 and Types L, N and H Mean for Your Project

By Mr Asphalt October 2026 8 min read

You open a set of civil drawings and find a note like "40 mm Size 10 Type H wearing course on 60 mm Size 20 Type SI". Most people nod and move on. But those few characters decide how the pavement performs, what it costs, how it gets tested, and who gets blamed when it ruts or ravels two years after handover.

This guide explains the asphalt mix types and asphalt mix sizes you'll see in Victorian tenders, based on the Department of Transport and Planning (DTP) Standard Section 407 Dense Graded Asphalt. It's written for architects, project managers and civil contractors who need to read a spec with confidence. It won't teach you to design a pavement. That's a job for a pavement engineer.

First, check you're reading the current spec

This catches people out more than anything else. The current Section 407 is version 18.0, released October 2025, replacing version 17.0. If your tender documents were built from an old template, they may call up mixes that no longer exist. For example, the July 2023 update removed Size 14 Type SI, yet it still appears in older specs.

The detailed descriptions of each mix type have also moved. Section 407 now refers readers to Code of Practice RC 500.01 for a description of the dense graded asphalt types. Many councils also adopt Section 407 with their own edits, so read the version attached to your contract, not the one you remember.

The number is the size

The number in a mix designation is the nominal aggregate size in millimetres. A bigger number means coarser stone, a coarser surface, and a thicker layer needed to compact it properly.

Size 7 is the fine end: thin layers, footpaths, bike paths and thin correction work. Size 10 is the everyday choice for residential streets, car parks and driveways. Size 14 is used for thicker wearing courses on busier roads. Size 20 is a structural mix that sits underneath and is rarely the surface you drive on.

The letter is the job

The letter shows what the mix is designed to handle. Types L, N, V and H are wearing course mixes, while the S series are structural mixes for intermediate and base courses. RC 500.01 describes them roughly like this:

Type L is a light duty Size 7 or 10 wearing course with low air voids and more binder, meant for very lightly trafficked pavements. Type N is light to medium duty in Sizes 7, 10 or 14, for light to moderate traffic. Type H is heavy duty in Sizes 7, 10 or 14, typically used mid-block on moderate to heavy traffic. Type V is a heavy duty Size 10 or 14 mix for moderate to heavily trafficked intersections.

There are also polymer modified versions. HP is a high performance mid-block mix in Size 10 or 14, and VP is a Size 14 mix for very heavily trafficked intersections, both built to resist deformation and cracking.

On the structural side, SI is a Size 20 intermediate course for heavy duty pavements or a base course in medium duty ones, and SF is a fatigue resistant Size 20 base course for heavy duty pavements with at least 175 mm of total asphalt.

Wearing course versus structural mix

The wearing course is the layer your tyres touch. Its job is skid resistance, ride quality and keeping water out of the pavement below. The structural layers carry and spread the load so the subgrade doesn't fail.

The mistake we see on smaller private jobs is treating the wearing course as the pavement. Putting 40 mm of a heavy duty surface over a weak or poorly compacted base won't save it. If the base moves, the surface cracks, whatever letter is on the drawing. The structure has to be designed for the traffic, and the wearing course is chosen to suit it.

Light versus heavy duty: what actually changes

People assume "heavy duty" just means "stronger". It's more specific than that. In the Austroads design method, Type L is designed at 50 gyratory cycles, Type N at 80 and Type H at 120. More lab compaction simulates more traffic, which pushes the design toward less binder and a stiffer, stonier mix.

That's great on a bus route. It's not so great on a quiet cul-de-sac. On lightly trafficked pavements, asphalt usually fails from age and weather (it dries out, cracks and ravels) rather than from rutting. A richer, more flexible Type L or N mix often lasts better there. Type H also tends to be harder to hand-work around pits and kerbs. This is practical experience, not a spec clause, but it's why specifying Type H everywhere "to be safe" can backfire.

The testing reflects the difference too. The rut test limit is tighter for 14H than for 10H, and tighter again for 14V, while Type L mixes are exempt from the modulus and wheel tracking tests.

When 10 mm or 14 mm gets chosen

Thickness comes first. Section 407 sets a minimum individual core thickness of 20 mm for Size 7, 25 mm for Size 10, 35 mm for Size 14 and 50 mm for Size 20. Those are acceptance minimums, not targets. In practice, crews are comfortable with Size 10 at around 30 to 40 mm and Size 14 at around 40 to 50 mm. That range is our industry estimate, so confirm it with your designer and supplier. If the drawings show 30 mm of Size 14, ask why.

Then consider traffic and turning stress. Size 14 offers more stone-on-stone contact, so it's the usual pick where trucks and buses are frequent, especially in thicker layers.

Detail work matters as well. Lots of kerb lines, pits, tight radii and hand-laid areas favour Size 10, which gives a neater finish at edges.

Appearance is worth a mention for architects. Size 10 gives a tighter, finer texture that suits forecourts and public spaces. Size 14 looks noticeably coarser.

Finally, think about tie-ins. Where new asphalt meets existing pavement, the chase is milled to a depth of 2.5 times the nominal size, with a minimum length of 600 mm at side streets, 3 m on roads of 80 km/h or less, and 6 m above that. A Size 14 tie-in means a deeper chase, which means more milling and cost.

The questions nobody answers in the tender briefing

Does "Type H" mean heavy vehicles are fine?

Not on its own. It describes the surface mix, not the pavement's load capacity. Heavy vehicle capacity comes from the full pavement design.

What about roundabouts and intersections?

Braking, turning and slow-moving trucks are what shove asphalt sideways. That's why Type V and VP exist. Using a mid-block mix in a busy intersection is a common cause of early shoving.

Is the mix actually registered?

A mix registration stays current for three years, as long as the aggregate sources, grading, filler sources and binder class don't change. Ask your supplier for the mix ID before work starts. It costs nothing and avoids an argument later.

Can we pave in a Victorian winter?

There are limits. For a wearing course using C170 or C320 bitumen, the pavement surface must be at least 10°C, rising to 15°C for C600 or polymer modified binders. Cold weather paving is allowed under conditions, but it needs Superintendent approval and a management plan. Allow for this in July programmes.

Is recycled content allowed?

Yes, within limits. Up to 5% recycled crushed glass sand is permitted in Type L, N, H, V, VP and HP mixes, but no RAP may be added to mixes containing polymer modified or EME2 binder. If your client has sustainability targets, don't write a blanket "no recycled material" clause.

How is compaction tested and paid?

Once the quantity of a given size and type goes above 300 tonnes, compaction must be tested on a lot basis. For layers under 50 mm thick, a lot is accepted at a characteristic density ratio of 95.0% or more, can be accepted at a reduced rate between 93.0% and 94.9%, and is removed and replaced at 92.9% or below. Contractors should price for this. Project managers should understand that a pay reduction is a contract outcome, not a favour.

Quick FAQs

What should I use for a driveway or residential car park?

For a light-traffic job, a Size 10 Type N or Type L is common, laid over a properly designed and compacted base. If delivery trucks or garbage trucks use it daily, have the pavement assessed rather than just bumping the surface up to Type H.

Is 14 mm stronger than 10 mm?

It resists rutting better in thicker layers, but the strength of the whole pavement comes from its structure, not the surface stone size.

Can Section 407 be used on private projects?

Yes, and it often is. But complete the schedule at clause 407.30, which sets out the course, size, type and thickness of each layer. A tender with blank schedules invites every tenderer to price something different.

What do SMA and OGA mean?

They're different mixes covered by their own sections. Stone mastic asphalt is in Section 404 and open graded asphalt is in Section 417. They don't fall under the L, N, H system.

A five-minute tender check

Before you issue or price a tender, check these five things:

01

The spec version is current.

02

Every layer has a size, type and thickness filled in.

03

The thicknesses suit the sizes.

04

Intersections use an intersection mix.

05

There's a pavement design behind the structural layers.

If any of those are missing, raise it at the RFI stage. It's far cheaper than raising it at the defects stage.

Our Satisfied Clients

<